Coated Rod for Soft Steel to 550 MPa Grade Steel Z-44【1-10 Pezzi per confezione】

Codice componente

Qui sono indicati i codici componente
correlati al prodotto ricercato

Codice componente
Z-44-2-2
Z-44-2-20
Z-44-2.6-5
Z-44-2.6-20
Z-44-3.2-20
Z-44-4-5
Z-44-4-20
Z-44-5-20
Codice componente
Prezzo unitario standard
Numero di pz. inclusi per conf.Quantità minima d'ordineSconto volumi elevati
Giorni
spedizione standard
?
Pole diameter
(mm)
Pole length
(mm)
Current range, lower
(A)
Current range, vertical position, elevating, upper Amount Of Content Mass
(g)

30.13 €

1 4 giorni 230030–6025~551 Case (2 kg)2000

195.35 €

10 Pezzi per confezione

1 conf. 8 giorni 230030–6025~551 Box (2 kg x 10 Cases)20000

64.68 €

1 4 giorni 2.635060–10050~901 Case (5 kg)5000

246.10 €

4 Pezzi per confezione

1 conf. 7 giorni 2.635060–10050~901 Box (5 kg x 4 Cases)20000

232.06 €

4 Pezzi per confezione

1 conf. 5 giorni 3.2350100–14090~1301 Box (5 kg x 4 Cases)20000

59.23 €

1 5 giorni 4450140~190120~1701 Case (5 kg)5000

158.81 €

4 Pezzi per confezione

1 conf. 5 giorni 4450140~190120~1701 Box (5 kg x 4 Cases)20000

157.36 €

4 Pezzi per confezione

1 conf. 8 giorni 5450190~250140~2101 Box (5 kg x 4 Cases)20000

Loading...

  1. 1

Informazioni di base

Product Type Barra per saldatura JIS Standard Z2311 E4303 Compatible Material Type For thin to medium plates, one of the representative brands
Application and Usage Characteristic Welding of general structures, such as vehicles, light gauge steel, and buildings. It reduces the amount of fumes by 30% compared to similar rods. With excellent re-arcing and slag removability, it is ideal for intermittent welding, fillet welding, and tack welding. It can be bent by hand for use, and with a rod diameter of 3.2 mm or less, vertical downward welding is also possible. Because it tends not to absorb moisture, under ordinary storage conditions, drying can be omitted. Main Points of Work Excessive current reduces X-ray performance and is the reason for degradation of workability. Hence, use the appropriate current range. Due to excessive absorption of moisture, besides deterioration of workability, pits may also occur. Hence, dehydrate at 70 to 100°C for 30 to 60 minutes. Due to excessive drying (for long period or high temperature), the penetration decreases, X-ray performance deteriorates and causes burning of the bar, even though there is no apparent change in quality. For medium and thick welding, adopt appropriate preheating / inter-path temperature. Chemical Composition of Deposited Metal C(%) 0.08
Chemical Composition of Deposited Metal Si(%) 0.14 Chemical Composition of Deposited Metal Mn(%) 0.34 Chemical Composition of Deposited Metal P(%) 0.014
Chemical Composition of Deposited Metal S(%) 0.009 Identification Color, Rod End Color Silver-gray color Identification Color, Secondary Color Blue White
Mechanical Properties of Weld Metal Proof Stress MPa 410 Mechanical Properties of Weld Metal Proof Stress, Tensile Strength MPa 460 Mechanical Properties of Weld Metal Proof Stress, Elongation(%) 28
Mechanical Properties of Weld Metal Proof Stress, Absorption Energy(J) 95 Authorized by the Classification Society of Japan NK,ABS,LR,DNV